MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.

Information provided by Braskem.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792/ISO 1183
  • Bulk Density, ASTM D-1895
  • Particle Size, ASTM D1921, Average; D50
  • Viscosity Test, ASTM D4020, Intrinsic
  • Molecular Weight, Braskem
  • Hardness, Shore D, ASTM D2240/ISO 868
  • Hardness, Shore D, ASTM D2240/ISO 868
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638/ISO 527
  • Elongation at Break, ASTM D638
  • Elongation at Break, ISO 527
  • Izod Impact, Notched, ASTM D256
  • Charpy Impact, Notched, ISO 11542-2, Determined with double-notched specimens
  • Coefficient of Friction, Dynamic, ASTM D1894
  • Coefficient of Friction, Static, ASTM D-1894
  • Abrasion, Braskem (sand slurry), reference Stainless Steel SAE1020 = 100
  • Abrasion, Braskem (sand slurry), ISO 15527 reference set as 100
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Heat of Fusion, ASTM D3418
  • CTE, linear, ASTM D696
  • Specific Heat Capacity, ASTM E1269
  • Thermal Conductivity, ASTM D177
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525/ISO 306
  • Melt Temperature, ASTM D3418
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.