An APE free, high strength sizing for glass and carbon fiber with excellent adhesion, providing good strand integrity and compatibility with most polyamide resins and polyester systems. Applications (properties imparted): Fiber Sizing (chopped strands, impact resistance, PA compatible, PET/PBT compatible, thermal stability). Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required. Information provided by Michelman |