MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LyondellBasell Astryn CA743GA Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: low melt flow, low modulus, UV-stabilized polypropylene copolymer with antiblock, good heat seamability, good puncture resistance, plasticizer-free, excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, pelletize resin

Applications: geomembranes, sheet

All ingredients meet TSCA (US) and DSL (Canada) registration requirements.

Description: Astryn CA74GA low melt flow, UV-stabilized, flexible polypropylene copolymer with antiblock is designed for geomembranes. It is based on proprietary Montell process technology and sheet made from it can be blown, slot die-extruded or calendared, with or without scrim, into a final form. This UV-stabilized, pelletized resin, when blended with an N-110 carbon black polyolefin carrier masterbatch to a concentration of 2.75% by weight carbon black in the finished product, provides exceptional weatherability. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors:
Available Properties
  • Density, ASTM D792B
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, 1% Secant, ASTM D790A, 0.05 in/min
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.