MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rogers Corporation RO3730 Antenna Grade Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of 0.0013 measured at 2.5 GHz. These values allow antenna designers to realize substantial gain values while minimizing signal loss. Materials are available with a demonstrated low PIM performance, with values better than -154 dBc (measured using Rogers' internal test method).

Cladding is 1 ounce rolled annealed copper (35 microns thick).

Features and Benefits:

  • RO3730 reinforced woven fiber glass with optimized glass and filler loading - Improved mechanical rigidity, easier handling and processing versus non-reinforced PTFE products and lower dissipation factor
  • Low PIM - reduced signal interference
  • Loss - improved antenna gain
  • Economically priced - volume manufacturing
  • Environmentally friendly - Lead-free process compatible and RoHS compliant

Typical Applications:

  • Base station antennas
  • RFID antennas
  • WLAN antennas
  • Satellite Radio antennas

Information provided by Rogers Corporation.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption at Equilibrium, ASTM D570, D48/50
  • Thickness, Range of Thicknesses Available
  • Flexural Strength, IPC-TM-650, 2.4.4, Y-Direction
  • Flexural Strength, IPC-TM-650, 2.4.4, X-Direction
  • Peel Strength, IPC-TM-650 2.4.8, Copper, After Solder Float
  • Volume Resistivity, IPC 2.5.17.1, Cond. A
  • Surface Resistance, IPC 2.5.17.1, Cond. A
  • Dielectric Constant, Differential Phase Length Method, Z direction, Design
  • Dielectric Constant, IPC-TM-650 2.5.5.5, Z direction, Process
  • Dissipation Factor, IPC-TM-650 2.5.5.5
  • Dissipation Factor, IPC-TM-650 2.5.5.5
  • CTE, linear, IPC-TM-650 2.4.41, X-Direction
  • CTE, linear, IPC-TM-650 2.4.41, Y-Direction
  • CTE, linear, IPC-TM-650 2.4.41, Z-Direction
  • Thermal Conductivity, IPC-TM-650, 2.6.2.1, D24/23
  • Decomposition Temperature, ASTM D3850
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.