MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Mallard Creek Polymers RoveneĀ® 6106 Styrene Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Rovene 6106 is a low viscosity but high solids letdown emulsion for paper and paper board substrates. The combination of the polymer design and high solids give inks formulated with Rovene 6106 very fast drying and excellent printability. The high solids, low viscosity, and fast drying characteristics are well suited for high speed gravure printing as well as flexographic printing.

Markets: Printing and Packaging

Applications: Printing Inks, Overprint Varnishes, Digital Inks and Coatings

Related Products: Rovene 6107, Rovene 4111, Rovene 6101, Rovene 4100, Rovene 5499

Information provided by Mallard Creek Polymers.

Vendors:
Available Properties
  • Solids Content
  • pH
  • Viscosity
  • Acid Value, Acid Number
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.