MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Master Bond Supreme 46HT-2 Toughened, High Shear and Peel Strength Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Supreme 46HT-2 is a two component epoxy adhesive featuring an attractive balance of good shear and peel strengths for high performance structural bonding and coating suitable for applications where long term exposure to temperatures from -100°F to +500°F is required. It is 100% reactive and does not contain any solvents or diluents. Supreme 46HT-2 is specially formulated to withstand rigorous thermal cycling and for bonding dissimilar substrates. The system cures rapidly at elevated temperatures at a minimum of 250°F. The mix ratio is 100 to 30-35 by weight. Unlike many other epoxy compounds, these strengths are relatively insensitive to small changes in the mix ratio. Supreme 46HT-2 can be applied by brushing or rolling. It produces durable, high strength, tough bonds which are resistant to thermal cycling as well as a wide variety of chemicals including water, many acids, bases, solvents, fuels and oils. Supreme 46HT-2 bonds well to most metals, ceramics, plastics and glass. It has excellent electrical insulation properties. The color of Part A is tan and the color of Part B is brown. Supreme 46HT-2 is widely used in aerospace, electronic, OEM and chemical/processing applications. A non-drip version called Supreme 46HT-2ND2 is also available that will not flow during cure. Both versions of this product are also readily available in black.

Product Advantages:

  • Convenient mixing: product properties relatively unaffected by small changes in mix ratio.
  • Easy application: contact pressure only required for cure, adhesive spreads evenly and smoothly.
  • Convenient cure schedules: Long pot life at room temperature. Requires an elevated temperature cure at 250°F minimum.
  • High bonding strength to similar and dissimilar substrates with superior peel strength.
  • Good durability, thermal shock and cycling capabilities.
  • 100% reactive and does not contain any solvents or diluents.
  • Excellent resistance to many acids, bases, solvents, fuels and petrochemicals.
  • Good electrical insulation properties.

Information provided by MasterBond®

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, Part A
  • Tensile Strength at Break
  • Shear Strength, Tensile lap, Al to Al
  • Shear Strength, Tensile lap, Al to Al, after 30 days water immersion
  • Peel Strength, T-peel, Al to Al
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Pot Life, 200 gram mass
  • Shelf Life, in original unopened container
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.