MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CHT Group QM 2325 25 Shore A, Condensation Cure Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QM 2325 is a two-component, room temperature, condensation cure, silicone material. The cured rubber is flexible and has excellent mechanical and physical properties in addition to good shelf-life stability. This material is an excellent choice for the molding of intricate patterns which involve deep undercuts and where dimensional stability becomes important while maintaining a fairly low modulus.

Key Features:

  • Low viscosity
  • Excellent tear resistance
  • Fast demold time
  • Moderately high durometer with a moderately low modulus
Main Applications:
  • Molds for large statues, small statues and monument restoration
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for technical articles and prototypes
  • Molds for architecture and picture frames

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors:
Available Properties
  • Specific Gravity, MM Cat 2300 Green, Uncatalyzed
  • Specific Gravity, MM Cat 2300 Green, Catalyzed
  • Specific Gravity, QM 2325, Uncatalyzed
  • Viscosity, MM Cat 2300 Green, Uncatalyzed
  • Viscosity, MM Cat 2300 Green, Catalyzed
  • Viscosity, QM 2325, Uncatalyzed
  • Linear Mold Shrinkage, Cured 3 days at 25°C
  • Hardness, Shore A, Cured 3 days at 25°C
  • Tensile Strength, Cured 3 days at 25°C
  • Elongation at Break, Cured 3 days at 25°C
  • Tear Strength, Cured 3 days at 25°C
  • Dry Time, MM Cat 2300 Green, Catalyzed
  • Cure Time
  • Tack-Free Time, MM Cat 2300 Green, Catalyzed
  • Pot Life, MM Cat 2300 Green, Catalyzed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.