Special Properties:• High wear resistance• Improved tensile and compressive strength• High temperature resistance• Extremely good fatigue strength• Low cold flow characteristics• Approved for use in the food industry (EU and FDA
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticPA, Polyamide