Introduction: These products are the raw material of polyurethane elastomers, coating, sealant, adhesive and chemical grouting material. They are mostly 2 or 3 functionality with different molecular weight from 400 to 5000. Applications: Can be used for polyurethane elastomer, waterproof coating, paving materials etc. Information provided by Shandong INOV Polyurethane Co., Ltd. |