Applications: Easy strippable insulation shielding compound for medium voltage power cables with rated voltage up to 35kV LUTENE® XL2710BK has excellent strippability, processability for medium voltage power cables (High viscosity version of XL2700BK). Characteristics: The advantage of LUTENE® XL2710BK over conventional strippable insulation shield compounds include: ? Consistent, clean adhesion level over -40 to 70? temperature range. ? Excellent extruded surface smoothness with fewer and smaller surface protrusions over broad range of shear rates. Specification: LUTENE® XL2710BK meets the property requirement of the following material specifications. ? AEIC CS8 ? ICEA S-94-649 ? IEC 60502 ? BS 6622 Information provided by LG Chemical |