MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
LyondellBasell Clyrell RC 124H Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC124H is a high modified polypropylene random copolymer designed for extrusion applications.

Clyrell RC124H exhibits enhanced optical properties. The main applications of Clyrell RC124H are blown film extrusion, sheet extrusion and thermoforming. Applications: Bags & Pouches, Food Packaging Film, Stationery Film, Textile Packaging Film

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Film Tensile Strength at Yield, MD, ASTM D882
  • Film Tensile Strength at Yield, MD, ASTM D882, 500 mm/min, Blown Film
  • Film Tensile Strength at Yield, TD, ASTM D882, 500 mm/min, Blown Film
  • Film Elongation at Break, MD, ASTM D 882
  • Film Elongation at Break, MD, ASTM D 882, 500 mm/min, Blown Film
  • Film Elongation at Break, TD, ASTM D 882, 500 mm/min, Blown Film
  • Film Elongation at Yield, MD, ASTM 882, 500 mm/min, blown film
  • Film Elongation at Yield, TD, ASTM 882, 500 mm/min, blown film
  • Secant Modulus, MD, ASTM D 882, 23 mm/min, blown film
  • Secant Modulus, TD, ASTM D 882, 23 mm/min, blown film
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, MD, ASTM D882, 500 mm/min, Blown Film
  • Film Tensile Strength at Break, TD, ASTM D882, 500 mm/min, Blown Film
  • 1% Secant Modulus, MD, ASTM D 882
  • Haze, ASTM D1003
  • Haze, ASTM D1003, laboratory blown film
  • Gloss, ASTM D 2457, 45°
  • Gloss, ASTM D 2457, @ 45°, laboratory blown film
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.