MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Premix Thermoplastics PREFLEX E50 Polyphenylene Ether (PPO/PPE)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material are available and marketed under the name PREBOARD. Thus the same material can also be used in rigid/flex boards. The material lends itself also well for injection moulding and is available for that purpose in granules sold under the name PREPERM. This enables the production of 3D circuit boards.
    Key features:
  • Low dissipation factor
  • Low dielectric constant
  • Low water absorption
  • High Tg
  • Zero shrinkage even at 190°C
  • Low CTE in all directions
  • Excellent adhesion with inks and adhesives
  • Excellent chemical resistance
  • Minimum thicknesses below 10 microns
  • Recyclable and RoHS compliant
  • Non halogen flame retardant grades also available
Applications: Flexible printed circuits, printed electronics, fuel cells and other uses calling for a special film.

Information from Premix OY

Vendors:
Available Properties
  • Density
  • Thickness
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Dielectric Constant
  • Dissipation Factor
  • Glass Transition Temp, Tg
  • Shrinkage, MD
  • Shrinkage, MD
  • Shrinkage, TD
  • Shrinkage, TD
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Premix Thermoplastics Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.