MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Evonik VARISOFT® 3690 PG (90%) Softener
Categories: Other Engineering Material

Material Notes: Composition: Imidazolinium compounds, 2-(C17 and C17-unsaturated alkyl)-1-[2-(C18 and C18- unsaturaded amido)ethyl]-4,5-dihydro-1-methyl, methyl sulfates in propylene glycol

Application:

  • VARISOFT® 3690 PG (90%) is a versatile textile softener for fabrics and garments.
  • VARISOFT® 3690 PG (90%) is a good coupler and co-emulsifier for cationic formulations.
  • VARISOFT® 3690 PG (90%) can be used to formulate highly concentrated dispersions.
Benefits:
  • VARISOFT® 3690 PG (90%) is a highly substantive cationic surfactant with weak emulsifying properties.
  • VARISOFT® 3690 PG (90%) does not contain a flammable solvent.
  • Goods treated with VARISOFT® 3690 PG (90%) have a smooth, non-greasy hand.
  • VARISOFT® 3690 PG (90%) is an effective antistat on polyester and cotton/polyester blends.
  • Goods treated with VARISOFT® 3690 PG (90%) have surprisingly excellent rewet properties. VARISOFT® 3690 PG (90%) can be used in combination with organomodified siloxane softeners such as TEGOPREN® 5884, TEGOPREN® 7008, TEGOPREN® 6924 and TEGO® EMULSION 4001 XP to impart a synergistic silicone softening effect and a non-greasy fatty hand effect.

Information provided by Evonik

Vendors:
Available Properties
  • Solids Content
  • pH, 10% in IPA/Water
  • Flash Point, PMCC
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.