MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Solaxis Ultem™ 9085 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM™ 9085 resin is a flame-retardant high-performance thermoplastic for digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high strength-to-weight ratio and its FST (flame, smoke and toxicity) rating. Combined with a Fortus® 3D Printer, ULTEM 9085 resin allows design and manufacturing engineers to produce fully functional parts that are ideal for advanced functional prototypes or end use without the cost or lead time of traditional tooling. Certified ULTEM 9085 meets more stringent test criteria and retains material traceability required by the aerospace industry. Certificates of Analysis for both raw material and filament are supplied, documenting test results and identification to match filament manufacturing lot number to raw material lot number. This allows traceability from printed part back to raw material.

Information provided by Solaxis Ingenious Manufacturing

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Moisture Absorption, ASTM E595, Loss during outgassing
  • Outgassing - Total Mass Loss, ASTM E595
  • Collected Volatile Condensable Material, ASTM E595
  • Tensile Strength, Ultimate, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Tensile Strength, Ultimate, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Tensile Strength, Yield, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Tensile Strength, Yield, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Elongation at Break, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Elongation at Break, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Elongation at Yield, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Elongation at Yield, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Tensile Modulus, ASTM D638, XZ Axis, Type 1, 0.2 in./min
  • Tensile Modulus, ASTM D638, ZX Axis, Type 1, 0.2 in./min
  • Flexural Strength, ASTM D790, ZX Axis, Method 1, 0.05 in./min
  • Flexural Strength, ASTM D790, XZ Axis, Method 1, 0.05 in./min
  • Flexural Modulus, ASTM D790, ZX Axis, Method 1, 0.05 in./min
  • Flexural Modulus, ASTM D790, XZ Axis, Method 1, 0.05 in./min
  • Flexural Strain at Break, ASTM D790, ZX Axis, Method 1, 0.05 in./min
  • Compressive Yield Strength, ASTM D695, ZX Axis, Method 1, 0.05"/min
  • Compressive Yield Strength, ASTM D695, XZ Axis, Method 1, 0.05"/min
  • Compressive Strength, ASTM D695, ZX Axis, Method 1, 0.05"/min
  • Compressive Strength, ASTM D695, XZ Axis, Method 1, 0.05"/min
  • Compressive Modulus, ASTM D695, ZX Axis, Method 1, 0.05"/min
  • Compressive Modulus, ASTM D695, XZ Axis, Method 1, 0.05"/min
  • Izod Impact, Notched, ASTM D256, ZX Axis, Method A
  • Izod Impact, Notched, ASTM D256, XZ Axis, Method A
  • Izod Impact, Unnotched, ASTM D256, ZX Axis, Method A
  • Izod Impact, Unnotched, ASTM D256, XZ Axis, Method A
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150-98
  • Dielectric Strength, ASTM D149-09, Method A
  • Dissipation Factor, ASTM D150-98
  • CTE, linear, ASTM E831
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Glass Transition Temp, Tg
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.