MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
BASF 3D Ultrafuse® PET Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Components: Amorphous Polyethylene Terephthalate based filament for Fused Filament Fabrication.

Product Description: Ultrafuse PET is made from a premium PET and prints as easy as PLA, but is much stronger. The filament has a large operating window for printing (temperature vs. speed), so it can be used on every 3D-printer. PET will give you outstanding printing results: a good layer adhesion, a high resolution and it is easy to handle. Ultrafuse PET can be 100% recycled, is watertight and has great colors and finish.

Information provided by BASF

Vendors:
Available Properties
  • Density, ISO 1183-1, Printed Part
  • Melt Flow, ISO 1133
  • Storage Temperature
  • Tensile Strength, ISO 527, ZX: Upright
  • Tensile Strength, ISO 527, XY: Flat
  • Elongation at Break, ISO 527, ZX: Upright
  • Elongation at Break, ISO 527, XY: Flat
  • Modulus of Elasticity, ISO 527, Young's, ZX: Upright
  • Modulus of Elasticity, ISO 527, Young's, XY: Flat
  • Flexural Strength, ISO 178, ZX: Upright
  • Flexural Strength, ISO 178, XY: Flat
  • Flexural Strength, ISO 178, XZ: On its edge
  • Flexural Modulus, ISO 178, ZX: Upright
  • Flexural Modulus, ISO 178, XZ: On its edge
  • Flexural Modulus, ISO 178, XY: Flat
  • Flexural Strain at Break, ISO 178, ZX: Upright
  • Flexural Strain at Break, ISO 178, XY: Flat
  • Flexural Strain at Break, ISO 178, XZ: On its edge
  • Izod Impact, Notched (ISO), ISO 180, ZX: Upright
  • Izod Impact, Notched (ISO), ISO 180, XZ: On its edge
  • Izod Impact, Notched (ISO), ISO 180, XY: Flat
  • Izod Impact, Unnotched (ISO), ISO 180, ZX: Upright
  • Izod Impact, Unnotched (ISO), ISO 180, XZ: On its edge
  • Izod Impact, Unnotched (ISO), ISO 180, XY: Flat
  • Charpy Impact Unnotched, ISO 179-2, ZX: Upright
  • Charpy Impact Unnotched, ISO 179-2, XZ: On its edge
  • Charpy Impact Unnotched, ISO 179-2, XY: Flat
  • Charpy Impact, Notched, ISO 179-2, ZX: Upright
  • Charpy Impact, Notched, ISO 179-2, XZ: On its edge
  • Charpy Impact, Notched, ISO 179-2, XY: Flat
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-2
  • Glass Transition Temp, Tg, ISO 11357-2
  • Processing Temperature, Bed, Bed Material: Glass
  • Nozzle Temperature
  • Drying Temperature, in a hot air dryer or vacuum oven
  • Dry Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.