MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Solvay EF5313 Polysiloxane Polymer
Categories: Polymer; Thermoset

Material Notes: Description: EF5313 is a back pigmented polysiloxane polymer prepreg matrix suitable for high temperature applications. EF5313 recommended cure is at 190°C (374°F), followed by a post-cure at 300°C (572°F). Typical applications include lightweight heat shields and ducts to protect composite structures for short durations up to 600°C (1112°F). The life of components made from EF5313 at elevated temperatures depends on the time, temperature and nature of the hot environment and must be determinded by in-situ testing. EF5313 is suitable for light-load bearing applications.

Features & Benefits:

  • 5 day tack life at 21°C (70°F)
  • 20 day tack life at 21°C (70°F) with both release films in position
  • 12 months storage at -18°C (0°F)
  • Autoclave processing
  • Typical cure 6 hrs at 190°C (374°F)
  • Suitable for high temperature applications
Note 1: Material: EF5313-6581 S2 glass fiber 300g/cm2; Cure: 6 hrs at 190° (374°F), 6.2 bar (90 psi); Post cure: 6 hrs at 300°C (572°F)
Note 1: Material: EF5313-6581 S2 glass fiber 300g/cm3. Quasi-isotropic laminate.; Cure: 6 hrs at 190° (374°F), 6.2 bar (90 psi); Post cure: 6 hrs at 300°C (572°F)

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, 6 hrs at 190°C, 90 psi + 6 hrs at 300°C
  • Storage Temperature
  • Tensile Strength, LIS/MEC/059, 0/90°, Note 1
  • Tensile Modulus, LIS/MEC/059, 0/90°, Note 1
  • Flexural Strength, LIS/MEC/250, 0/90°, Note 1, Exposure: 1 hr at 600°C
  • Flexural Strength, LIS/MEC/250, 0/90°, Note 1, Exposure: 1 hr at 400°C
  • Flexural Strength, LIS/MEC/250, 0/90°, Note 1
  • Flexural Modulus, LIS/MEC/250, 0/90°, Note 1, Exposure: 1 hr at 600°C
  • Flexural Modulus, LIS/MEC/250, 0/90°, Note 1, Exposure: 1 hr at 400°C
  • Flexural Modulus, LIS/MEC/250, 0/90°, Note 1
  • Shear Strength, LIS/MEC/252, 0/90° Interlaminar. Note 1
  • Maximum Service Temperature, Air, short term
  • Cure Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.