MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Matexcel ANT-0053 Conductive touch screen gloves finishing agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Conductive touch screen gloves agent is a finishing agent that gives textiles a certain conductivity. The treated leather, textiles, etc. have good conductivity, so that touch screen mobile phones and other electronic devices can be operated without taking off the gloves, which solves the problem of having to take off the gloves when answering calls or operating electronic devices outdoors in cold winter. ·Good conductivity, high transparency, without changing the original color of fabric or leather; ·Good resistance stability, not affected by temperature and humidity, stable and reliable performance; ·The feel of the leather and fabrics will not be affected after finishing, ensuring the original flexibility and elasticity; ·Safe and environmentally friendly, non-toxic to human body, no side effects.

Application: It can be used for conductive finishing of glove fabrics such as leather, chemical fiber, blended and pure cotton. It is usually used for the conductive treatment of the index finger of gloves to achieve the effect of operating the touch screen without taking off the fabric.

Morphology: Blue transparent liquid

Uses: Can be treated by padding and dipping, without dilution, and used directly. -Padding process: padding ? drying (80-100°C, 2-3 minutes) ? baking (130-170°C, adjust according to the temperature resistance of the fabric); -Impregnation process: fabric ? impregnation (soak evenly) ? dehydration (recover the thrown solution and add it to the impregnation tank) ? drying (130-170°C, adjust according to the temperature resistance of the fabric).

Key Words: Conductive touch screen gloves finishing agent
Vendors:
Available Properties
  • Storage Temperature, Storage in a cool, dry place, avoid direct sunlight.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.