MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chesterton 633 SXCM Synthetic, Extreme Pressure & Corrosion Resistant Grease-with Moly
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 633 Synthetic Extreme Pressure & Corrosion Resistant Grease with Moly is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse with outstanding extreme pressure and anti-wear capabilities, shear stability, temperature and corrosion resistance. As a premium quality, water resistant grease, 633 will not be removed even in severe water washout situations. Chesterton 633 can be used in steam and direct water contact services. With a dropping point of 288°C (550°F). It will not melt and run out even at high speeds or under heavy loads as found in Mining, Metal Processing, Steel, Aluminum or Copper Manufacturing Industry. 633 SXCM is greatin its ability to extend bearing life, reduce equipment repairs and improve operational efficiency of grease lubricated equipment. It is especially advantageous where there is exposure to high humidity, corrosive vapors and shock loading or vibration as found in pulp and paper mills, mining operations, power generating plants, steel mills and metal forming operations. Applications include the lubrication of pinch roll and press roll bearings, dryer and calendar roll bearings, corrugators and sitters, blowers and fan bearings, oven conveyors bearings, cranes and mechanical presses.

Features:

  • Virtually impervious to water and steam
  • Synthetic Base Fluid
  • Compatible with most elastomers and seals
  • Smooth Tack Texture
  • Adheres to Metal
  • Outstanding Extreme Pressure Resistance
  • Water and Corrosion Resistant
  • Wide temperature range.

Suggested Uses: Use in all applications where conventional grease break down under shear, thermal abuse, shock loading and water contamination. Chesterton 633 SXCM can be used whenever thermally stable grease is required.

Applications:

  • Slides, guides, plain bearings and bushings.
  • Anti-friction bearings, roller bearings and ball bearings
  • Kiln Ring, Shoe and Rollers
  • Couplings, joints and splined shafts
  • Mining Equipment,Off Road
  • Cranes, Drag Lines
  • Railways, Switch Gear and Curve Lubrication

Lubricating Additives: Non Heavy Metal, Extreme Pressure and Anti-Wear, Anti-Fretting Additives, Surface Reactive Anti-Rust and Corrosion Additives, Oxidation Inhibitors

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity Measurement, ASTM D445, Base Oil
  • Kinematic Viscosity at 40°C (104°F), ASTM D445, Base Oil
  • Kinematic Viscosity at 100°C (212°F), ASTM D445, Base Oil
  • Four Ball Extreme Pressure, Load Wear Index, ASTM D2596, DIN 51 350/4
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596, DIN 51 350/4
  • Four Ball Wear, ASTM D2266, DIN 51 350/5, 1200 rpm, 40 kg, scar diameter
  • Penetration, ASTM D217, DIN ISO 2137
  • Timken Test, ASTM D2509
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Dropping Point, ASTM D2265, DIN 51 801/1
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.