MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Solvay Capran® 980 Vacuum bagging film
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Vacuum bagging film. Ideally suited to heavy industrial applications.

Features & Benefits:

  • Clear, heat-stabilized, cast film produced from a modified nylon resin
  • It is a cast film recommended as a gagging film for advanced composite fabrication, transparence laminating and other high-temperature applications where dimensional stability and uniform film gauge are essential
  • In addition, It has excellent heat stability and resistance to pin holes
  • It can be used in cure cycles up to 205°C (400°F). It can be heat seamed to meet any custom shape requirements.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Thickness
  • Thickness
  • Thickness
  • Thickness
  • Tensile Strength, ASTM D882
  • Elongation at Break, ASTM D882
  • Tensile Modulus
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.