MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Henkel Loctite® Stycast® 2762FT with CAT 14 Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 2762FT provides the following product characteristics:
  • High temperature resistance
  • High thermal conductivity
  • Excellent chemical resistance
  • Low coefficient of thermal expansion
  • Low shrinkage

Cure: Room temperature or Heat cure

Application: Potting, Encapsulant

Loctite Stycast 2762FT epoxy encapsulant is designed for potting electronic components exposed to harsh environments. This material is also ideal for large and complex castings that require high temperature resistance and thermal conductivity.

Loctite Stycast 2762FT can be used with a variety of catalysts.

CATALYST DESCRIPTION

Loctite CAT 14 provides the following product characteristics:

  • Powdered epoxy hardener
  • Chemical resistant
  • High temperature performance
  • Long work life

Cure: Heat cure

Information provided by Henkel.

Vendors:
Available Properties
  • Density, Mixed
  • Density, Part A, Loctite Stycast 2762FT
  • Brookfield Viscosity, Part A, Loctite Stycast 2762FT
  • Hardness, Shore D
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Working Life, 100 g
  • Shelf Life, Part A, Loctite Stycast 2762FT
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.