MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Copper nickel 10%, UNS C70600, H55 Temper, Tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Light Drawn, Light Cold Rolled

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Butt Weld; Good Suitability – Coated Metal Arc Welding, Spot Weld, Seam Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding

Common Fabrication Processes: Forming and Bending; Welding

Typical uses: Brake Lines; Power Steering Tube; Screw Lamp Bases; Condenser Plates; Condensers; Distiller Tubes; Evaporator Tubes; Evaporators; Ferrules; Heat Exchanger Tubes; Pressure Vessels; Pump Impellers for Oil Refining; Valve Bodies; Weld Torch Tips; Boat Hulls; Hot Water Tanks; Propeller Sleeves; Salt Water Baffles; Salt Water Piling Wrap; Salt Water Pipe Fittings; Salt Water Piping Systems; Ship Hulls; Tube Sheet for Salt Water Service; Water Hoses; Flanges

Applicable Specifications: Bar – Rolled ASTM B122/B122M, ASTM B151/B151M, MILITARY MIL-C-15726; Condenser & Heat Exchanger Tube with Integral Fins – ASTM B956/B956M; Pipe – ASTM B466/B466M, ASTM B467, ASME SB467, ASME SB466; Plate – ASTM B432, Condenser Tube ASME SB171, MILITARY MIL-C-15726, ASTM B122/B122M, Condenser Tube SAE J463, Condenser Tube SAE J461, Condenser Tube ASTM B171/B171M; Rod – Welding AWS A5.15, ASTM B151/B151M, MILITARY MIL-C-15726; Sheet – SAE J461, MILITARY MIL-C-15726, SAE J463, ASTM B122/B122M; Strip – ASTM B122/B122M, MILITARY MIL-C-15726; Tube - Condenser Tube ASTM B552, Condenser Tube SAE J463, Condenser Tube ASME SB111, MILITARY MIL-T-22214, Condenser Tube MILITARY MIL-T-15005, Condenser Tube ASTM B111/B111M, ASTM B543/B543M, MILITARY MIL-T-16420, ASME SB543, MILITARY MIL-T-16420, ASME SB395, Condenser Tube SAE J461, ASTM B359/B359M, ASTM B469, ASME SB466, ASTM B466/B466M, ASME SB359, ASTM B395/B395M; Wire – MILITARY MIL-C-15726

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B
  • Hardness, Rockwell F
  • Hardness, Rockwell 30T
  • Tensile Strength, for Standard
  • Elongation at Break
  • Tensile Modulus
  • Modulus of Rigidity
  • Poissons Ratio, Calculated
  • Machinability
  • Electrical Resistivity, 9% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Point
  • Hot-Working Temperature
  • Copper, Cu, As Balance
  • Iron, Fe
  • Lead, Pb
  • Manganese, Mn
  • Nickel, Ni
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.