MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GY-FR-C80 Flame Retard Coating/ Fireproof Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Applying GY-FR-C80 SERIES on the base material can offer products permanently and excellent flame retard effect.

Intro: Innovative GY-FR-C80 SERIES is developed regarding fireproof demanding from all walks of life. GY-FR-C80 SERIES also make the textile functional series more completed. GY-FR-C80 can offer products permanently and excellent flame retard effect. GY-FR-C80 SERIES can be applied on fiber, textile, leather, wood, polymer, various kinds of industries and life products to meet your needs for fireproof and enhance additional value for products.

Advantages:

  • GY-FR-C80 SERIES can offer various based material products excellent fireproof effect.
  • GY-FR-C80 SERIES are non-halogen and without heavy mental that can meet the ROSH standard.
  • GY-FR-C80 SERIES can use in various material and fiber fabric.
  • GY-FR-C80 SERIES can enhance the physical properties of the product, including the tearing resistance, elasticity and wear resistance.
  • GY-FR-C80 SERIES have permanent flame retard effect.
  • Confer permanent and excellent feel for fabric and textile.
  • With excellent weather resistance and anti-UV, applied to various kinds of interior and outdoor products.
  • Combining GY-FR-C80 SERIES with GOYENCHEM- 744 on products can reach flame retard and water/oil repellent multi- functions.
  • GY-FR-C80 SERIES are easy to apply and convenient processibility.
  • Combining GY-FR-C80 SERIES with GY-MF-PU-(dipping type fireproof additive) can reach multi effects of flame retard on surface and fireproof in fabric.
Applications:
  • GY-FR-C80 SERIES is post-processing special flame retardant, can apply on all kinds of synthetic fabric and enhance additional value for products.
  • GY-FR-C80 SERIES can apply on various flexible and rigid materials.
  • GY-FR-C80 SERIES can use in Polyester, Nylon, PP, Rayon, Cotton.
  • GY-FR-C80 SERIES can apply on various fireproof coating of materials.
  • Apply in flame retardant paper coating for papermaking industry.
  • Use in related natural leather and synthetic leather flame retard process.
  • Apply in different flame retardant fabric: non-woven, Brushing Fabric,knitting fabric, twilletc.
  • Treat as textile flame retardant back adhesive, flam retardant adhesive layer and other post-treatment use.
  • Applications for flame retardant functional fabrics: various kinds of flame retard industrial fabric, flame retardant curtain, fire resisting fiber, industrial zipper, tent fabric, baby seat fabric.
  • Excellent weather resistance make it apply on interior upholstery and various kinds of outdoor products.

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • pH
  • Viscosity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.