MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Henkel Loctite® ABLESTIK 285 CAT 11 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Black

Mix Ratio, by weight -Material:Catalyst: 100:4

Mix Ratio, by Volume -Material:Catalyst: 100:9.9

Product Benefits:

  • Thermally conductive
  • Non-sag
  • Thixotropic
  • Resin versatility
  • Low CTE
  • Long pot life
  • Good chemical resistance
  • Good physical and chemical properties at elevated temperatures
Cure: Heat cure

Application: Thermally conductive adhesive

Typical Assembly Applications: Bonding metals and ceramic substrates in heat sink applications

LOCTITE ABLESTIK 285 CAT 11 adhesive is designed for assembly applications that require thermal management. It is also recommended for low stress bonding applications. LOCTITE ABLESTIK 285 CAT 11 can be used with a variety of catalysts.

Information provided by Loctite®

Vendors:
Available Properties
  • Density, Mixed Properties
  • Density, Part A Properties 285
  • Viscosity, Part B Properties CAT 11
  • Outgassing - Total Mass Loss, ASTM E 595, per NASA Reference Publication 1124, Sample cured for 8 hours @ 82°C
  • Collected Volatile Condensable Material, ASTM E 595, per NASA Reference Publication 1124, Sample cured for 8 hours @ 82°C
  • Shear Strength, ASTM D1002, Lap, Aluminum to aluminum
  • Shear Strength, ASTM D1002, Lap, Aluminum to aluminum
  • Shear Strength, ASTM D1002, Lap, Aluminum to aluminum
  • Volume Resistivity, ASTM D257, Cured
  • Dielectric Constant, ASTM D150, Cured
  • Dielectric Strength, ASTM D149, Cured
  • Dissipation Factor, ASTM D150, Cured
  • CTE, linear, ASTM D3386, Cured
  • Thermal Conductivity, ASTM D-2214, Cured
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, ASTM D3418, Cured
  • Cure Time
  • Cure Time
  • Cure Time
  • Working Life, Mixed Properties, 100 g mass
  • Shelf Life, Part A Properties 285
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Loctite Division of Henkel

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.