Temper: Nominal Grain Size 0.050 mm Fabrication Properties: Excellent Suitability - Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability - Oxyacetylene Welding, Butt Weld Common Fabrication Processes: Blanking; Coining; Coppersmithing; Drawing; Etching; Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; Piercing and Punching; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping Typical Uses: Air Lines; Gasoline Lines; Hydraulic Lines; Oil Lines; Air Conditioner Tubes and Condenser Sheets; Gas Lines; Heater Lines; Heater Lines; Heather Units; Oil Burner Tubes; Air Conditioners; Refrigerators; Air Lines in Airplanes; Brewery Tubes; Casting Molds; Condenser Tubes; Dairy Tubes; Distiller Tubes; Evaporator Tubes; Gage Lines; Gasoline Lines in Airplanes; Heat Exchanger Tubes; Hydraulic Lines in Airplanes; Kettles; Oil Coolers in Airplanes; Oil Lines in Airplanes; Paper Liens; Plating Anodes; Plating Hangers; Plating Racks; Plumbing Tube; Pulp Lines; Rotating Bands; Steam Lines; Tanks; Water Lines; Oil Coolers; Oil Lines; Plumbing Fittings; Plumbing Pipe |