MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance values of 1010 O with PRE-ELEC® (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved. The products made out of these PRE-ELEC® ESD products are washable, reusable and recyclable. The grade is designed for injection molding of transparent parts. In addition, PRE-ELEC® ESD 5350 can be used in clean applications with extremely low amount of extractable ions. The melt flow property of PRE-ELEC® ESD 5350 is tailored to fit the requirements of injection molding. PRE-ELEC® ESD 5350 is RoHS compliant.

Applications: Bins and other injection molded parts, where permanent ESD protection and high cleanliness are required. The product can be used mainly in electronics packaging, but in many other application areas as well.

Processing: PRE-ELEC® ESD 5350 compound can be processed in normal processing conditions as with polypropylene.
Test Specimen: 10[mm] wide moulded rod

Information from Premix OY

Vendors:
Available Properties
  • Density
  • Thickness
  • Linear Mold Shrinkage, ISO 294-4
  • Melt Flow, ISO 1133
  • Tensile Strength, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • Surface Resistance, ISO IEC 61340-5-1
  • Static Decay, ISO IEC 61340-5-1
  • Deflection Temperature at 0.46 MPa (66 psi), 75/Method Bf
  • Deflection Temperature at 1.8 MPa (264 psi), 75/Method Af
  • Transmission, Visible, transparent; thickness not quantified
  • Zone 1, Cylinder
  • Zone 1, Die
  • Zone 2, Cylinder
  • Zone 2, Die
  • Zone 3, Die
  • Zone 3, Cylinder
  • Zone 4, Die
  • Zone 4, Cylinder
  • Zone 5, Die
  • Zone 5, Cylinder
  • Melt Temperature
  • Mold Temperature
  • Roll Temperature, 2nd Roll
  • Roll Temperature, 3rd Roll
  • Roll Temperature, 1st Roll
  • Drying Temperature, Pre-drying in a dehumidifier
  • Dry Time
  • Injection Pressure
  • Shelf Life, Normal Storing Conditions
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Premix Thermoplastics Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.