Available Properties |
---|
- Specific Gravity, JIS-K-6220; ASTM D-792
- Specific Gravity, JIS-K-6220, 120°C for 1,000 hrs
- Specific Gravity, JIS-K-6220, 150°C for 1,000 hrs with 90% RH
- Specific Gravity, JIS-K-6220, 60°C for 1,000 hrs with 90% RH
- Specific Gravity, JIS-K-6220, 70°C for 1,000 hrs
- Hardness, Shore C, SRIS0101
- Hardness, Shore C, SRIS0101, 150°C for 1,000 hrs with 90% RH
- Hardness, Shore C, SRIS0101, 60°C for 1,000 hrs with 90% RH
- Hardness, Shore C, SRIS0101, 70°C for 1,000 hrs
- Hardness, Shore C, SRIS0101, 150°C for 1,000 hrs
- Hardness, Shore OO, ASTM D2240
- Tensile Strength, Yield, JIS-K-6251(#2), 120°C for 1,000 hrs
- Tensile Strength, Yield, JIS-K-6251(#2)/ASTM D-412
- Tensile Strength, Yield, JIS-K-6251(#2), 70°C for 1,000 hrs
- Tensile Strength, Yield, JIS-K-6251(#2), 150°C for 1,000 hrs with 90% RH
- Tensile Strength, Yield, JIS-K-6251(#2), 60°C for 1,000 hrs with 90% RH
- Elongation at Yield, JIS-K-6251(#2), 120°C for 1,000 hrs
- Elongation at Yield, JIS-K-6251(#2)/ASTM D-412
- Elongation at Yield, JIS-K-6251(#2), 70°C for 1,000 hrs
- Elongation at Yield, JIS-K-6251(#2), 150°C for 1,000 hrs with 90% RH
- Elongation at Yield, JIS-K-6251(#2), 60°C for 1,000 hrs with 90% RH
- Tear Strength, JIS-K-6252 (Angle), 150°C for 1,000 hrs with 90% RH
- Tear Strength, JIS-K-6252 (Angle), 120°C for 1,000 hrs
- Tear Strength, JIS-K-6252 (Angle), 70°C for 1,000 hrs
- Tear Strength, JIS-K-6252 (Angle)/ASTM D-624
- Tear Strength, JIS-K-6252, 60°C for 1,000 hrs with 90% RH
- Volume Resistivity, JIS-K-6249, 60°C for 1,000 hrs with 90% RH
- Volume Resistivity, JIS-K-6249, 70°C for 1,000 hrs
- Volume Resistivity, JIS-K-6249/ASTM D257
- Volume Resistivity, JIS-K-6249, 150°C for 1,000 hrs with 90% RH
- Volume Resistivity, JIS-K-6249, 120°C for 1,000 hrs
- Dielectric Strength, JIS-K-6249; ASTM D-149
- Dielectric Strength, JIS-K-6249, 120°C for 1,000 hrs
- Dielectric Strength, JIS-K-6249, 150°C for 1,000 hrs with 90% RH
- Dielectric Strength, JIS-K-6249, 60°C for 1,000 hrs with 90% RH
- Dielectric Strength, JIS-K-6249, 70°C for 1,000 hrs
- Dielectric Breakdown, JIS-K-6249; ASTM D-149, Withstand Voltage [V/min]
- Thermal Conductivity, JIS-R-2618; ASTM D2326
- Thermal Conductivity, JIS-R-2618, 120°C for 1,000 hrs
- Thermal Conductivity, JIS-R-2618, 150°C for 1,000 hrs with 90% RH
- Thermal Conductivity, JIS-R-2618, 60°C for 1,000 hrs with 90% RH
- Thermal Conductivity, JIS-R-2618, 70°C for 1,000 hrs
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
| | |