MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Unifrax Fiberfrax® PH Blanket Ceramic Fiber Insulator
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax PH blanket is a unique product that has been specifically designed to provide excellent filtration capabilities in addition to the high chemical stability and low thermal conductivity that is possessed by all Fiberfrax products.

PH blanket is made from Fiberfrax bulk ceramic fibers in a unique wet felting process which removes unfiberized particles. In addition to the strength and resiliency afforded by the interlocking of fibers during the manufacturing process, handling strength is further enhanced by the addition of a small amount of organic binder.

A typical filtration application would involve utilizing PH blanket as a platinum catalyst recovery filter in nitric acid production. In this application, PH blanket offers numerous advantages over glass woll products including longer life, 50-60% improved filter efficiency, reduced chance of blowouts, and better temperature resistance.

    Typical Applications
  • Catalyst recovery filter in nitric acid production
  • Diffusion medium for fluidized beds
  • Filtration and catalyst carrier medium for radioactive particles and hot exhaust gases

Information Provided by Unifrax I LLC

Vendors:
Available Properties
  • Density
  • Melting Point
  • Maximum Service Temperature, Air, Recommended Operating Temperature
  • Al2O3
  • SiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Unifrax I LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.