MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik VESTAMID® L2124 black 9.7507 | PA12 Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: High viscosity, plasticized, heat and light stabilized PA12 Compound. VESTAMID® L2124 black 9.7507 is a plasticized, heat- and light- stabilized polyamide 12 compound for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications. Tubing according to DIN 73 378, Type: PA 12-PHL. Properties of compounds based on PA 12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® L2124 natural colored is characterized by a high melt viscosity and good dimensional control during pipe extrusion. VESTAMID® L2124 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values.

Property data for dry samples unless otherwise noted.

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Density, ISO 1183, Conditioned
  • Moisture Absorption, Sim. to ISO 62
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Strength, Yield, ISO 527, Conditioned
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Conditioned. Nominal
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Yield, ISO 527, Conditioned
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Tensile Modulus, ISO 527, Conditioned
  • 50% Modulus, ISO 527
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179/1eA, Complete Break
  • Charpy Impact, Notched, ISO 179/1eA, Complete Break, Conditioned
  • Charpy Impact, Notched, ISO 179/1eA, Partial Break
  • Tensile Creep Modulus, 1 hour, ISO 899-1
  • Tensile Creep Modulus, 1000 hours, ISO 899-1
  • Volume Resistivity, IEC 62631-3-1, Conditioned
  • Volume Resistivity, IEC 62631-3-1
  • Surface Resistance, IEC 62631-3-2
  • Dielectric Constant, IEC 60243-1
  • Dielectric Constant, IEC 60243-1, Conditioned
  • Dielectric Constant, IEC 60243-1
  • Dielectric Constant, IEC 60243-1, Conditioned
  • Dielectric Strength, IEC 60243-1, AC, S20/P50
  • Dielectric Strength, IEC 60243-1, AC, S20/P50
  • Dissipation Factor, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1, Conditioned
  • Dissipation Factor, IEC 62631-2-1
  • Dissipation Factor, IEC 62631-2-1, Conditioned
  • Comparative Tracking Index, IEC 60112, Test solution A, 100 drops value. Conditioned
  • Comparative Tracking Index, IEC 60112, test solution A, 50 drops value
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, Method B: 10 N, 50 K/h
  • Vicat Softening Point, ISO 306, Method A: 10 N, 50 K/h
  • Flammability Test, IEC 60695-11-10
  • Flammability Test, IEC 60695-11-10
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.