MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Nouryon Perkadox L-40 RPS Dibenzoyl peroxide
Categories: Other Engineering Material

Material Notes: Perkadox L-40 RPS is a special peroxide formulation containing 40% benzoyl peroxide which disperses and dissolves very quickly in pure unsaturated polyester and acrylic resins. The product is specially developed for curing road-marking acrylic coatings and fits high pressure machines presently used in road marking. The product carries the approval from leading spraying machine equipment manufacturer in Germany. It has excellent storage stability. The fine particle size allows for fast dissolving.

CAS number: 94-36-0, 78-40-0

EINECS/ELINCS No.: 202-327-6; 201-114-5

Applications: Perkadox L-40 RPS is a pumpable, sprayable easy dispersing form of dibenzoyl peroxide for the curing of unsaturated polyester resins at ambient and elevated temperatures. At cure-temperatures up to 80°C, Perkadox L-40 RPS should be used in combination with an aromatic tertiary amine accelerator, above 80°C the use of an accelerator is not required. Perkadox L-40 RPS can be pumped through internal and external mix FRP spray equipment and poured or metered by volume, Perkadox L-40 RPS is easier to use and handle than conventional dibenzoyl peroxide pastes or dispersions. The low water content of Perkadox L-40 RPS allows for use in all FRP applications.

Information provided by Nouryon

Vendors:
Available Properties
  • Density
  • Viscosity, Ericksen
  • Molecular Weight
  • Storage Temperature
  • Decomposition Temperature, Self-Accelerating Decomposition Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.