MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Foam Grade

Material Notes: Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed cell structure does not absorb water and acts as a water barrier. Because of its staple pull and screw pull strength, Celtec Marine is ideal for applications in marine upholstery, seat backs, seat bottoms, trim for rough fiberglass openings, brackets, cabinets, draws etc.

FEATURES AND BENEFITS

  • Light weight- Celtec marine combines lightweight with strength to reduce weight in boat construction.
  • Strength- Celtec Marine has a high strength to weight ratio that makes it ideal for many boat building applications.
  • Superior workability- Celtec marine is easy to form, cut, glue, screw, nail, and staple.
  • Flammability- Celtec Marine meets UL guidelines, is self extinguishing and has a flame spread of 20.
  • Thermal conductivity- Celtec Marine is an excellent insulator.
  • Weatherability and water resistance- Celtec Marine is durable and will not absorb water.
  • Density- Celtec Marine is lighter than water and it floats.
  • Safety- Celtec Marine is Lead, cadmium, barium and zinc free.
  • Stability- Celtec Marine will not rot and it is cleanable and retains its color.
  • Economical- Celtec Marine is designed to last and it is economical to use.

Information provided by Compression Polymers Corp - Vycom

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Tensile Strength, Ultimate, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Charpy Impact, Unnotched, ASTM D256, [ft-lb/in]
  • Gardner Impact, ASTM D4228
  • CTE, linear, ASTM D696
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flame Spread Index, ASTM E84
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CPC - Vycom Co. Compression Plastics Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.