MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chemours Teflon® PTFE Grade 304A Aqueous Dispersion  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon® PTFE 304A fluoropolymer resin is a negatively charged, hydrophobic colloid containing approximately 45% (by total weight) of 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles suspended in water. A milky white liquid, Teflon® PTFE 304A also contains approximately 6% (by weight of PTFE) of a nonionic wetting agent and stabilizer. It also contains a thickening agent to increase the viscosity and ethylene glycol to retard evaporation of the water and give a level coating. The viscosity at room temperature is around 1700 cP as measured on a Brookfield viscometer using a #1 spindle at 60 rpm. The viscosity of Teflon® PTFE 304A is very non-Newtonian. Measurement of the viscosity at lower spindle speeds will give higher viscosity values.

The pH of Teflon® PTFE 304A is normally above 9.5.

When properly processed, the PTFE resin in Teflon® PTFE 304A exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

Teflon® PTFE 304A is normally used to coat gaskets. In many cases, a thick coating is applied, which is heated to remove the ethylene glycol and wetting agents but is not sintered. The thick coating cold flows when the gasket is tightened. This helps ensure a tight seal in addition to the benefits of easy removal of the gasket due to the nonstick nature of PTFE.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors:
Available Properties
  • Specific Gravity, ASTM D4441
  • Base Resin Density, ASTM D4441, Weight of PTFE resin solids
  • Solids Content, ASTM D4441, Percent of PTFE resin solids
  • Particle Size, Average dispersion particle size
  • pH, ASTM E70
  • Viscosity, ASTM D2196
  • Melting Point, ASTM D1457
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Chemours, former DuPont

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.