MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Petropol Nypol® A3 G35 HS UV RH PRTA010 NR346 Nylon 66, 35% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Product Description: 35% Glass Fiber, Hydrolysis Resistant and Heat Stabilized Polyamide 66

Resin ID (ISO 1043): PA66 GF35
Additive: Heat Stabilized
Processing: Injection Molding
Color: Black
Data: VW 50133; VW 501 27; FIAT 55232

Information provided by Petropol

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, ISO 62, Equilibrium
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Ash, SO 3451-1/A
  • Hardness, Rockwell R, ISO 2039
  • Tensile Stress, ISO 527
  • Elongation at Break, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Modulus, ISO 527
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • Charpy Impact, Notched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Melting Point, ISO 3451-1/A
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  • Processing Temperature, Molding
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Ensinger PEI
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.