- Continuous Tinning Flux for Copper Wire and Strip
- Zinc-Free, Chloride Activated, Organic Acid Formulation
- Designed for Continuous Tinning of Heavy Gage Copper Wire
- Does Complete Tinning of Strip or Wire Surfaces with a Single Pass
- Completely Water-based Formulation, No Solvents and No Alcohols
Description: Superior No. 462 is a zinc-free, halide-activated, organic acid type flux for continuous tinning of copper wire and strip. The acidity of the Superior No. 462 comes from organic acid, as a result it is much less corrosive to tinning equipment than inorganic acid and zinc chloride based fluxes. Superior No. 462 leaves minimal, zinc-free residue in the tinning pot after tinning.Applications: Superior No. 462 was formulated for the continuous tinning of copper wire and strip. The activity of this flux allows it to work on heavy gage wire that typically is tinned at high speeds. Normal flux application such as total immersion of the copper wire or strip is recommended. Non-continuous applications will work by adding flux by part immersion or by brush. Information provided by Superior Flux |