Dow Polypropylene Homopolymer Resins are semi-crystalline thermoplastic materials that can provide a combination of desirable properties and affordability: low density; excellent chemical resistance and ESCR; excellent moisture barrier; high heat resistance, good gloss; high stiffness and hardness, and low water absorption. Dow Polypropylene Homopolymer resins are suitable for a wide range of applications and may be fabricated by injection molding, blow molding and extrusion. H705-04Z Polypropylene Homopolymer resin for extrusion and injection molding, offers improved heat resistance. Data provided by Dow Chemical. Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product. |