MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Röhm ACRYLITE® 16 mm Alltop Acrylic Double-Skin Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: 16 mm ACRYLITER Alltop acrylic double-skin sheet is a light transmitting, heat-insulating and weather-resistant double-skinned sheet made of acrylic (polymethyl methacrylate, PMMA) polymer with particularly wide rib spacing. It was designed for commercial & institutional greenhouses where an extremely high light transmission is required.

Advantages of 16 mm ACRYLITE® Alltop UVA/UVT acrylic double-skin sheet

  • ACRYLITE® Alltop has a light transmission of 91%, the 64 mm wide flute is the highest light transmitting of any insulating rigid glazing available.
  • ACRYLITE® Alltop‘s patented no drip coating is applied on every surface, including inside the flutes. The coating allows for maximum light transmission virtually eliminating all condensation droplets on all interior and exterior surfaces of the sheet.
  • Better plant growth response is driven by high light transmision and the option for ACRYLITER Alltop in UV absorbing or UV transmitting is available.
  • Up to 50% better energy savings over single layer glazings.
  • Better plant growth response is driven by the light transmission and the option of ACRYLITER Alltop UV absorbing or UV transmitting is available.

    Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

  • Vendors:
    Available Properties
    • Thickness
    • CTE, linear
    • Thermal Conductivity
    • Maximum Service Temperature, Air
    • Smoke Density, ASTM D2843
    • Ignition Temperature, ASTM D1929, Autoignition
    • Transmission, Visible
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Röhm GmbH , former product of Evonik Corporation; Evonik Cyro

    Category Notes
    Plastic

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Proto3000 – 3D Engineering Solutions
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.