1. fast curing; 2. high level of detail and sharp contours; 3. smooth and dry object surface; 4. low odor Description: Type D Flex Black is used for 3D printers, using DLP or LCD/LED (DUP) technologies. This datasheet describes the technical properties and application of the resin. Safety aspects are described in the according safety data sheet. The resin is filled in HDPE bottles with UN-approval for transportation (UN 3H1/x1.9/250). Each bottle carries a sticker indicating the according signs on hazards from the content, gives a link to the safety data sheet and indicates the track ID of the production LOT and expiration date. Information provided by DruckWege GmbH |