MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Dover Chemical MAYCO BASE RP 8765 Dicarboxylic Acid Salt Based Compound Synthetic Corrosion Inhibitor
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Mayco Base RP-8765 is a corrosion inhibitor formulated for use in synthetic and semi-synthetic metalworking coolants. It can be utilized in both oil-absorbing and oil-rejecting synthetic fluid types. It is completely water soluble in all proportions, yielding very light-colored transparent solution. As opposed to other corrosion inhibitors, Mayco Base RP-8765 also brings a slight amount of lubricity to the formulated product. Mayco Base RP-8765 can be formulated into: Synthetic rust preventatives for in-process protection. Rust inhibitors for coolant tank-side additions. Inhibition packages for synthetic and semi-synthetic fluids Used at 12% concentration in the following grinding coolant, Mayco Base RP-8765 exhibits complete rust protection to a 33:1 dilution in 100ppm water.

Information provided by DoverChem

Vendors:
Available Properties
  • Specific Gravity, 60/60°F
  • Density
  • pH, 5% concentration
  • pH, Neat
  • Total Acid Number, [meqHCl/g]
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.