MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Derived from annually renewable resources, RenewTech™ BioPlastics 7000 sheet is made with Ingeo™ PLA biopolymer as a base, giving you a packaging solution with competitive cost value performance compared to traditional materials. RenewTech 7000 complies with FDA and European requirements for food packaging.

Characteristics:
Made from annually renewable resources
Improved environmental footprint (requires less non-renewable energy and generates significantly less greenhouse gas)
Excellent flavor and aroma barrier
Superior print and lamination
High gloss
Stones allows for down gauging
Food contact approved
Superior visual qualities
High modulus
Compostable

End Uses:
Food packaging
Organic in-store prepared food packaging
Thermoformed hinged packaging
Tray packaging

Information provided by Ex-Tech Plastics Inc.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Tensile Strength at Break, ASTM D882
  • Tensile Strength, Yield, ASTM D882
  • Elongation at Break, ASTM D882
  • Tensile Modulus, ASTM D882
  • Izod Impact, Notched, ASTM D256
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.