Perkadox 14-40K-PD-S is a 40% formulation on an inert carrier system (main carrier clay) in powder form. CAS number: 2212-81-9, 25155-25-3 EINECS/ELINCS No.: 218-664-7 Applications: Perkadox 14-40K-PD-S is a bifunctional peroxide which is used for the crosslinking of natural rubber and synthetic rubbers, as well as polyolefins. Rubber compounds containing Perkadox 14-40K-PD-S have excellent scorch safety, and under certain conditions one step mixing is possible. Safe processing temperature: 135°C (rheometer ts2 > 20 min.). Typical crosslinking temperature: 175°C (rheometer t90 about 12 min.). Information provided by Nouryon |