MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Saint-Gobain Tygon® PT-3350 Sanitary Silicone Tubing Formulation
Categories: Polymer; Thermoset; Silicone

Material Notes: Tygon® 3350: Designed for high-purity applications, Tygon® Sanitary Silicone Tubing's ultra-smooth inner bore can reduce the risk of particle entrapment and microscopic buildup during sensitive fluid transfer. In-house analysis of the inner surface of Tygon® Sanitary Silicone Tubing compared to other silicone tubing shows that it is up to three times smoother. Additionally, this smoother fluid path facilitates complete system cleaning and sterilization. Utilizing a platinum-curing process, Tygon® Sanitary Silicone Tubing eliminates the concern of extraction often encountered when alternative curing methods are used. It has also been fully characterized using the ISO 10993 standards, reducing user cost and time associated with process validation.

Features/Benefits:
  • Ultra-smooth inner bore reduces potential for particle entrapment
  • Minimal extractables help maintain fluid integrity
  • Documented biocompatibility for sensitive applications
  • Excellent fluid flow characteristics
  • Fully tested to ISO 10993 standards to facilitate validation process
Typical applications include Pharmaceutical and Cosmetic Processing, Medical Devices, Cell Harvest and Media Process Systems, Sterile Fill Lines, Water for Injection (WFI) Transfer, Chemistry and Blood Analyzers, Liquid Chromatography.
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792-91
  • Water Absorption, ASTM D570-81, 24 hours at 23°C
  • Hardness, Shore A, ASTM D2240-91, 15 seconds
  • Tensile Strength, Yield, ASTM D412-92
  • Elongation at Break, ASTM D412-92
  • 200% Modulus, ASTM D412-92
  • Tear Strength, ASTM D624-91 Die B, Initial Tear Strength
  • Compression Set, ASTM D395-89 Method B, Constant Deflection, for 22 hrs.
  • Compression Set, ASTM D395-89 Method B, Constant Deflection, for 22 hrs.
  • Dielectric Strength, ASTM D149-93
  • Maximum Service Temperature, Air
  • Brittleness Temperature, ASTM D746-79
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.