MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
AK Steel 409 ULTRA FORM® Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and roping in both automotive exhaust and non-exhaust applications. These benefits are achieved through precise control of chemistry and thermo-mechanical processing from melting to finishing. AK Steel 409 ULTRA FORM is essentially non-hardenable by heat treatment because of its titanium and low-carbon levels. The titanium additions not only stabilize the steel to prevent hardening during welding, but also prevent the formation of harmful chromium carbides which can lead to intergranular corrosion in service.
Available Forms
AK Steel produces 409 ULTRA FORM Stainless Steel coils and cut lengths in thicknesses of 0.015" to 0.250" (0.381 to 6.350 mm) in widths up to and including 48" (1219 mm). For applications over 0.120" (3.048mm) thick, AK Steel 409 Ni Stainless Steel will provide improved toughness and weldability. The surface finish of the alloy is obtained by annealing and pickling after rolling. The pickled surface is relatively dull and, like other titanium-stabilized stainless steels, may have cosmetic titanium streaks and will appear similar to typical Type 409.

Information provided by AK Steel.

Key Words: UNS S40920
Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Annealed
  • Hardness, Rockwell B, 5% Cold Worked
  • Hardness, Rockwell B, 10% Cold Worked
  • Hardness, Rockwell B, 50% Cold Worked
  • Hardness, Rockwell B, 15% Cold Worked
  • Hardness, Rockwell B, 30% Cold Worked
  • Hardness, Rockwell B, Annealed, Transverse Orientation
  • Tensile Strength, Ultimate, 5% Cold Worked
  • Tensile Strength, Ultimate, 10% Cold Worked
  • Tensile Strength, Ultimate, 15% Cold Worked
  • Tensile Strength, Ultimate, 30% Cold Worked
  • Tensile Strength, Ultimate, 50% Cold Worked
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, Annealed, Transverse Orientation
  • Tensile Strength, Yield, Annealed, Transverse Orientation, 0.05"-0.085"
  • Tensile Strength, Yield, 5% Cold Worked
  • Tensile Strength, Yield, 10% Cold Worked
  • Tensile Strength, Yield, 15% Cold Worked
  • Tensile Strength, Yield, 30% Cold Worked
  • Tensile Strength, Yield, 50% Cold Worked
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, 50% Cold Worked, in 2"
  • Elongation at Break, 30% Cold Worked, in 2"
  • Elongation at Break, 15% Cold Worked, in 2"
  • Elongation at Break, 10% Cold Worked, in 2"
  • Elongation at Break, 5% Cold Worked, in 2"
  • Elongation at Break, Annealed, in 2"
  • Elongation at Break, Annealed, Transverse Orientation
  • Tensile Modulus
  • Fatigue Strength, r=0.1
  • Fatigue Strength, r=0.1
  • Electrical Resistivity
  • Carbon, C, Ti, min. = 8X(C+N)
  • Chromium, Cr
  • Iron, Fe, as balance
  • Manganese, Mn
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.