MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
ExxonMobil Ronex MP
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Exxon RONEX MP is a premium quality multipurpose grease that can be used in a wide range of automotive and industrial applications. RONEX MP consists of a mineral oil base fluid thickened with a lithium complex soap thickener, and contains performance-enhancing additives. RONEX MP grease has excellent performance over a wide temperature range, and provides moderate load carrying and extreme pressure properties. In addition it is resistant to water, and provides protection against corrosion. The grease has good oxidation and thermal stability. RONEX MP is compatible with most elastomer seal materials. RONEX MP is an NLGI Grade 2 grease. RONEX MP grease may be used in industrial applications in bearings, gears and couplings that require the use of water resistant, extreme pressure grease. It may also be used in electric motors of the NEMA insulation Class A and B types. RONEX MP is an excellent all round automotive grease, it can be used as a chassis grease for extended lubrication intervals, as well as a wheel bearing grease. The high thermal stability of the grease means that it is ideally suited to wheel bearings of disc brake vehicles, where high temperatures are generated during severe braking. RONEX MP can also be used as a lubricant for ball joints, as it provides good protection from wear, low torque, and protection against water contamination. RONEX MP meets the NLGI GC-LB requirements for wheel bearings and chassis lubrication. RONEX MP has become the grease of choice for many users, especially those with multiple grease applications.

Application notes: RONEX MP is recommended for application by hand packing or by grease gun. It should not be used in centralised lubrication systems having long feeder lines unless these systems are designed to handle a Grade 2 consistency grease. RONEX MP is a multi-purpose grease for both industrial and automotive applications operating in a wide range of conditions of temperature, loading and environment. Specific applications include: Industrial - All kinds of plain and rolling element bearings; Industrial - Couplings and gears; Industrial - Electric motors of the NEMA (National Electric Manufacturers Association) Insulation Class A and B types; Automotive - Truck, bus and construction applications; Automotive - Wheel bearings, especially those operating at high temperature, for instance during severe braking with disc brakes; Automotive - Ball joints and chassis lubrication

Key Words: NLGI Grade 2
Vendors:
Available Properties
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Oxidative Stability, ASTM D942, Pressure Drop of 69 kPa
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear, ASTM D2266
  • Penetration, ASTM D217, Worked, 25°C
  • Timken Test
  • Dropping Point, ASTM D2265
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.