MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Beryllium Copper 21C UNS C82510 Casting Alloy Solution Treated and Aged
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: The 1% Co content is a good grain refiner, and as a result, this alloy is used instead of beryllium-copper alloys C82500 and C23400 when thin sections must be cast at high temperatures or when thick and thin sections are present within the same casting in order to achieve a uniform fine-grained structure. The higher cobalt content imparts better wear resistance but less desirable polishability and machinability. Typical uses are comparable to those of beryllium-copper alloys C82500 and C23400.

Test specimen: solution treated at 790 to 800°C and aged 3 hours at 345°C.

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm
  • Modulus of Elasticity
  • Poissons Ratio
  • Machinability, UNS C36000 (free-cutting brass) = 100%
  • Shear Modulus
  • Electrical Resistivity, 20% IACS, as-cast tempers
  • Magnetic Permeability
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point, Incipient
  • Melting Point
  • Solidus
  • Liquidus
  • Solution Temperature
  • Aging Temperature
  • Casting Temperature, Heavy castings
  • Casting Temperature, Light castings
  • Aluminum, Al
  • Beryllium, Be
  • Chromium, Cr
  • Cobalt, Co
  • Copper, Cu
  • Iron, Fe
  • Lead, Pb
  • Nickel, Ni
  • Silicon, Si
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.