MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Lubrizol Advanced Materials Stat-Rite® S-506 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product Description: S-506 is a static dissipative High-Impact Polystyrene alloy. It utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to enhance standard HIPS packaging sheet with a layer of clean, permanent ESD protection. Used as a skin layer, Stat-Rite® S-506 provides more consistent ESD protection than coatings and anti-stat. The Stat-Rite® skin will NOT wash off or deteriorate over time, providing reliable ESD protection for many years. Features: More permanent than anti-stat; Provides protection for many years; Cleaner than anti-stat, coatings or carbon-filled sheet; More consistent than anti-stat or coatings. Applications: Static dissipative layer on HIPS electronics packaging.
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Rapid Static Decay; Wear Resistant
Uses: Electrical/Electronic Applications; Packaging
Appearance: Yellow
Forms: Pellets

Information provided by Lubrizol Advanced Materials, Inc.

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Tensile Strength, Yield, ASTM D638, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  • Elongation at Break, ASTM D638, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  • Tensile Modulus, ASTM D638, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  • Flexural Modulus, ASTM D790, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  • Surface Resistance, ESD S11.11, 12% RH, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  • Surface Resistivity per Square, ASTM D257, 50% RH, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Merquinsa

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.