MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GOYENCHEM-HGC High Strength Green Material
Categories: Other Engineering Material

Material Notes: GOYENCEHM-HGC is a high strength green material that can be reacted by water. Through stirring process, this material is easy to be molded into various shapes.

Features:

  • Fast drying: Can be took out from molds in 15-45 minutes
  • Easy to use : Can be diluted with water directly
  • Environment-friendly: Use recycled waste and reduce pollution.
  • Improve heat insulation effect
  • Fireproof to prevent spread of fire disaster
  • Heat resistance
  • Will not blister, smoke or chip after burning
  • Will not crack or deformation
  • Anti-quake: Use lot of waste of agriculture life material and decrease weight of construction
  • Nail and screw are available use : Can be drilled by nail or screw
Applications:
  • Green Residence
  • 3D print
  • Commercial Building
  • VILLA
  • Medical Building
  • Military buildings
  • Carved panels
  • Furniture material
  • Break water
  • Can be used as a sealant or adhesion
  • Use as surface treatment , also can be sprayed on the surface

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Volatiles
  • Melting Point
  • Cure Time
  • Cure Time, Functional Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.