MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Phillips 66 CVT Fluid Full-Synthetic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Kendall® CVT Fluid is a premium quality, full-synthetic transmission fluid specifically designed for use in passenger cars with belt-driven continuously variable transmissions. It has been specifically engineered to have the unique frictional properties required for use in this type transmission. CVT Fluid has carefully balanced frictional properties to protect against belt slippage and wear while also providing excellent anti-shudder performance. It has high shear stability and excellent oxidation resistance for long service life. It helps protect against sludge and varnish formation, and has excellent low-temperature properties for easier shifting in cold weather. The synthetic formulation provides enhanced performance benefits at extreme temperatures compared with conventional, all-mineral transmission fluids. CVT Fluid is recommended for most Honda, Jeep, Mitsubishi, Nissan (except Altima hybrid) and Suzuki vehicles with CVT transmissions. It is not recommended for eCVT or chain-driven CVT transmissions, or in any non-CVT transmission. Please refer to the owner’s manual for correct transmission fluid recommendation.

Applications:

  • Passenger cars with belt-driven continuously variable transmissions (CVTs)
Features/Benefits:
  • Meets performance requirements for nearly all vehicles with belt-type continuously variable transmissions
  • High steel-on-steel friction to prevent belt slippage, which can result in high or even catastrophic wear
  • Low steel-on-paper friction to prevent torque converter clutch slippage, which can result in shudder
  • Excellent oxidation resistance and thermal stability for long fluid life
  • Protects against sludge and varnish formation
  • Protects against wear
  • Protects against rust and corrosion
  • Excellent low-temperature properties for easier shifting in cold weather
  • Good seal compatibility
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Brookfield Viscosity
  • Viscosity Measurement, Index
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.