MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Premix Thermoplastics PRESEALĀ® TPE 6071
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: PRESEAL TPE 6071 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasketing and grounding applications. Conductivity is achieved with a silver coated glass sphere and fiber combination. PRESEAL TPE 6071 can be extruded like an ordinary thermoplastic elastomer thus giving great new possibilities in mass production. It has adhesion to selected thermoplastics, which opens construction possibilities with co-extrusion e.g. in making combined weather/dust/EMI gaskets. Recyclability is an added value. The material is silicone free.

Typical applications include EMI gaskets in mobile phones, mobile phone

* Tension test bar according to ISO 527 base stations and other wireless communication environment as well as in military applications.

Information provided by Premix Thermoplastics Inc.

Vendors:
Available Properties
  • Density
  • Hardness, Shore A, ISO 7619
  • Tensile Strength, Ultimate, ISO 37*
  • Tensile Strength, Yield, ISO 37*
  • Elongation at Break, ISO 37*
  • Elongation at Yield, ISO 37*
  • Modulus of Elasticity, ISO 178
  • Compressive Modulus, ISO 7743, At 10% Compression
  • Compressive Modulus, ISO 7743, At 15% Compression
  • Compressive Modulus, ISO 7743, At 18% Compression
  • Tear Strength, ISO 34-C
  • Compression Set, ISO 815:1991
  • Volume Resistivity, ISO Mil-G-835388
  • Shielding Effectiveness, ISO ARP1705, 20-700 MHz
  • Middle Barrel Temperature, Zone 2; Cylinder
  • Middle Barrel Temperature, Zone 1; Cylinder
  • Middle Barrel Temperature, Zone 3; Cylinder
  • Middle Barrel Temperature, Zone 4; Cylinder
  • Middle Barrel Temperature, Zone 5; Cylinder
  • Middle Barrel Temperature, Zone 6; Cylinder
  • Die Temperature, Zones 1-5
  • Drying Temperature, Pre-drying; If stored for longer than 1 year
  • Moisture Content, When Produced
  • Shelf Life, Normal Storing Conditions
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Premix Thermoplastics Inc.

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.