MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Phillips 66 Bentone NLGI Grade 2
Categories: Fluid; Lubricant; Clay Gellant

Material Notes: Bentone is a high-quality, extreme-pressure (EP), clay-thickened grease developed for the lubrication of industrial equipment operating under heavy loads and at high temperatures. It is particularly recommended for medium-to-large, low-speed bearings operating at very high temperatures where conventional soap-based greases typically fail to provide satisfactory lubrication. Bentone is manufactured with high-quality, heavy paraffinic base oils and a non-soap, bentonite clay thickener. It is fortified with extreme-pressure and antiwear additives to provide outstanding protection for bearings and moving parts exposed to heavy loads and high operating temperatures. It retains its consistency at high temperatures and has good water washout resistance and good storage stability.

Applications:

  • Banbury mixers
  • Drying ovens
  • Jaw crushers
  • Kiln cars
  • Rolling and strip mills
  • Steel mills
  • Aluminum, cement, glass and rubber plants
Features/Benefits:
  • Non-melt clay thickener
  • Excellent resistance to changes in consistency at high temperatures
  • Good extreme-pressure and antiwear properties
  • Adheres to metallic surfaces
  • Good shear stability
  • High film strength
  • Resists water washout
  • Good mechanical and storage stability

Information provided by Phillips 66 Lubricants.

Vendors:
Available Properties
  • Density
  • Viscosity Measurement, Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Oxidative Stability, ASTM D942, Pressure Drop
  • Four Ball Extreme Pressure, Load Wear Index
  • Four Ball Extreme Pressure, Weld Load, ASTM D2596
  • Four Ball Wear
  • Penetration P(60), 1/10 mm, ASTM D217
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point, (Base Oil Property)
  • Dropping Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.