MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Jilin Xingyun Chemical 1502 Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Characteristics: The shelf of styrene butadiene rubber is longer because of its good stability. The property of styrene butadiene rubber is similar to that of natural rubber. It will appear physical and chemical change, while its oxidization is slow under the effect of light, heat, oxygen and ozone. More filling agents can be added in styrene butadiene rubber and hardly affect the physical and mechanical properties of styrene butadiene rubber, therefore, styrene butadiene rubber is fit for the production of rubber products with lower content of rubber. The low temperature resistance and resilience of styrene butadiene rubber is not as good as natural rubber, but styrene butadiene rubber is better than natural rubber as for antifriction, heat-proof, oil proof and resistance to aging.

Usage: 1500 type styrene butadiene rubber is use for tire, sidewall rubber, general back rubber, line belt, sebific duct sole and other black rubber products with excellent physical properties, and without limit to pollution and color. 1502 type styrene butadiene rubber is used for white sidewall rubber, hosepipe, galoshes, sole, rubber fabric and clothes, toys and black and colorful products with excellent physical properties and nopollution.1712 type styrene butadiene rubber is use for tread of tire, line belt, back rubber, rubber coated wire, cable and general black industrial products. 1778 type styrene butadiene rubber is used for light-colored and transparent products such as light-colored sidewall rubber, sebific duct, line belt, fabric and clothes, galoshes, sole, medicinal product and sports goods, toys and others.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors:
Available Properties
  • Volatiles, Superior grade
  • Volatiles, Grade 1
  • Volatiles, On-spec
  • Mooney Viscosity, Superior grade, ML 1+4
  • Mooney Viscosity, Grade 1 and On-spec, ML 1+4
  • Mooney Viscosity, ML 1+4
  • Ash
  • Tensile Strength at Break, Grade 1, On-spec
  • Tensile Strength at Break, Superior grade
  • 300% Modulus, Grade 1, On-spec
  • 300% Modulus, Superior grade
  • 300% Modulus, Superior grade
  • 300% Modulus, Grade 1, On-spec
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.