MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Dover Chemical MAYSOL SSD50 Semi-Synthetic Coolant Concentrate Bio-Stable Semi-Synthetic Base
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Maysol SSD-50 is a semi-synthetic coolant concentrate that allows the formulator to blend a high quality, general-purpose product. Applications that can be performed with Maysol SSD-50 range from light duty to medium duty on both ferrous and non-ferrous operations. Such operations may include grinding, milling, turning, and drilling. Maysol SSD-50 is recommended to be blended with water, preferably soft or deionized, at a mix of 50/50, before delivery to your customer. If these water conditions are not available at your location, it is recommended to make a small lab blend to ensure clarity and stability of the concentrate and subsequent emulsion. Maysol SSD-50 is fully fortified with biocide, corrosion inhibitors, and wetting agents. If a chlorinated version of the product is desired, Paroil 53-NR can be added up to 5% by weight to the concentrate before blending back with the water. To produce a non-chlorinated EP version, the addition of Maylube S-830, up to 15% by weight, can be added after the blend back with water. This product is to be kept from freezing.

Information provided by DoverChem

Vendors:
Available Properties
  • Specific Gravity, 60/60°F
  • Density
  • pH, 5% concentration
  • pH, Neat
  • Saybolt Viscosity at 100°F
  • Kinematic Viscosity at 40°C (104°F)
  • Total Acid Number, [meqHCl/g]
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.